Trade Name and Grade:PA66 HAP001 Improved impact strength |
Properties | Test Standard | Test condition | Unit | Typical Value |
Mechanical properties |
Tensile strength | ISO527 | 5mm/min | MPa | 65 |
Tensile Stain,Break | ISO527 | 5mm/min | % | 28 |
Flexural strength | ISO178 | 2mm/min | MPa | 85 |
Flexural modulus | ISO178 | 2mm/min | MPa | 2100 |
Charpy notched impact strength | ISO179-1eA | 23℃ | KJ/m2 | 7.5 |
Hardness | IOS2039 | 23℃ | N/mm2 | 100 |
Thermal properties |
Heat distortion temperature | ISO 75 | 1.8MPa | ℃ | 66 |
Heat distortion temperature | ISO 75 | 0.45MPa | ℃ | 170 |
Physical properties |
Density | ISO1183 | 23℃ | g/cm3 | 1.13 |
Other properties |
Molding Shrinkage | ISO2577 | / | % | 1.2-1.7 |
Address:No.369, Guangming Road, Zhuangshi Street, Zhenghai District, Ningbo. |
Tel:(0574)87244771 Fax:(0574)87241375 |
These technical data in the product brochures are typical data under specific test conditions( at 23±2℃ and 50±5% relative humidity) and not intended foruse as limiting specifications. |